3M
Adhesives, Tapes, and Fastening Solutions
3M offers a broad portfolio of industrial bonding, fastening, and assembly technologies. The portfolio includes Scotch-Weld™ structural epoxy, polyurethane, and acrylic adhesives; VHB™ acrylic foam tapes; Dual Lock™ reclosable fasteners; and a wide selection of transfer, foam, and specialty tapes. These products support demanding applications across electronics, transportation, industrial fabrication, and general manufacturing. Compatible nozzles, applicators, and dispensing equipment are also available to support controlled material preparation and application.
As an authorized 3M distributor, Krayden supplies a broad selection of Scotch-Weld, VHB, Dual Lock, and Fastbond™ products, along with compatible application equipment. Our team also provides technical guidance to help customers evaluate materials, substrates, application requirements, and dispensing processes.
Markets Served by 3M
Featured 3M Brands
Explore four core 3M brands covering structural adhesives, acrylic foam tapes, reclosable fasteners, and contact adhesives.

Scotch-Weld™
Structural epoxy, polyurethane, and acrylic adhesives for bonding metals, composites, engineering plastics, and other industrial substrates.

VHB™
High-strength acrylic foam tapes that can replace mechanical fasteners or liquid adhesives in suitable permanent-bonding applications.

Dual Lock™
Mushroom-profile reclosable fasteners designed for removable panels, access covers, components, and other repeated-access assemblies.

Fastbond™
Contact and pressure-sensitive adhesives for bonding foam, fabric, laminates, and other flexible or lightweight materials.
Structural & Engineering Adhesives
Scotch-Weld structural adhesives are two-part, high-performance bonding systems used to join metals, composites, and engineering plastics where mechanical fasteners or welding are not practical. The line spans epoxy, urethane, and acrylic chemistries suited to different substrate combinations, cure speeds, and environmental demands. Packaging and required mix ratios vary by product. Selected systems are supplied in Duo-Pak cartridges or bulk containers and may use 1:1, 1:2, 10:1, or other product-specific mixing configurations. Confirm the specified mix ratio and equipment compatibility for the exact adhesive before use.
Industrial Tapes
3M's tape portfolio ranges from permanent structural bonding tapes to temporary transfer adhesives, foam cushioning tapes, and specialty conductive or shielding tapes. VHB tapes are engineered to replace fasteners and liquid adhesives entirely, while transfer and ATG tapes offer fast, mess-free lamination for graphics, gaskets, and componentry.
Spray, Contact, & Hot Melt Adhesives
3M spray, contact, and hot melt adhesives support assembly processes ranging from broad-area coverage and flexible-material bonding to rapid-set production applications. Selecting the appropriate technology depends on the substrates, required open or set time, application method, production rate, and expected service conditions.
3M Reclosable Fasteners
3M reclosable fastening systems include Dual Lock mushroom-profile fasteners, click straps, and conventional hook-and-loop products for removable panels, access covers, components, and repeated-access assemblies. System selection depends on the desired closure strength, reopening frequency, attachment surface, environmental exposure, and installation method.
Application Equipment & Accessories
3M application equipment includes static mixing nozzles, manual and pneumatic adhesive dispensers, and dedicated ATG tape applicators. Equipment must be matched to the product format, cartridge volume, mix ratio, connection interface, desired dispense rate, and production method to support controlled, repeatable application.
Talk to our Experts
Whether you need material selection support, help matching a Scotch-Weld chemistry to your substrates, or guidance on dispensing equipment for your production line, our team can help you find the right 3M solution for your application.
3M Quick Reference
302 products
-
-
-
3M™ Scotch-Weld™ Structural Polyurethane Adhesive DP609
- Rapid room-temperature curing
- Flexible structural bonding
- Approx. 9-minute work life at 23°C
-
-
3M DP8010
- Ability to structurally bond polyolefins without special surface preparation
- Excellent water and humidity resistance
- One step process
-
3M 74
- Used for bonding flexible urethane or latex foam
- Provides excellent coverage.
- Soft, non-dimpling glue lines.
-
3M™ Repositionable Spray Adhesive 75
- Provides "tape-like" bonds
- Bonds paper, cardboard, acetate, foil, fabrics, etc.
- Extra-long tack range
-
-
-
-
-
-
3M™ Double Sided Tape 415
- Double Sided Acrylic Adhesive
- Good adhesion to various substrates
- Excellent for indoor / outdoor applications
-
-
Scotch® ATG Transfer Tape 924
- Thin 0.002 in. (0.05 mm) profile for low-profile bonding
- Reverse wound construction for use with ATG hand-held dispensers
- Provides consistent and controlled adhesive application
-
Scotch® ATG Transfer Tape 926
- Provides immediate and permanent bonds with high adhesion
- Excellent performance up to 450 ºF (232 ºC)
- Adheres to a variety of substrates (ABS, acrylic, PP, PE, etc.)
-
Scotch® ATG Transfer Tape 969
- Provides immediate and permanent bond
- Designed to adhere to a variety of substrates
- Conforms easily to curves and contours
-
3M™ Double-Sided Paper Tape 9086
- Bonds to a wide variety of substrates
- 0.5 mil tissue carrier
- Double coated with 3.5 mil adhesive on each side
-
3M 9485PC
- Utilizes a fiber-reinforced adhesive for roll stability
- Resistance to humidity, water, solvent, and chemicals
- The 5 mil (127µm) thick version of 3M™ Adhesive Transfer Tape 9482PC
-
3M™ Removable and Repositionable Double-Sided Tape 9415PC
- Features a removable, repositionable, low-tack adhesive
- Withstands temperatures as low as -20 °F (-29 °C) and as high as 158 °F (70 °C)
- Ideal for temporary mounting of lightweight materials
-
3M F9473PC
- Transparent, double sided, 10 mil (0.26 mm) VHB™ transfer tape
- Short term temperature tolerance of up to 500 °F (260 °C)
- Operating temperature tolerance of up to 300°F (149°C)
-
3M™ VHB™ Tape 4910F
- Clear Double Sided Tape
- Acrylic Adhesive
- Permanent Bonding for High Surface Energy Substrates
-
-
-
3M 4026
- Provides strong holding power for long-term performance
- Maintains bond integrity under elevated temperatures
- Adapts to uneven or irregular surfaces
-
3M 4032
- Provides durable, long-term holding power
- Flexible and conformable for bonding on irregular surfaces
- Foam structure reduces vibration and enhances stability
-
3M™ Double Sided Foam Tape 9528
- Rubber adhesive delivers quick “grab” for fast bonding
- Adhesive on both sides for easy mounting and joining
- Provides light conformability and consistent thickness
-
3M™ VHB™ Tape GPH-110GF
- High Temperature Performance (Up to 230°C)
- Permanent seal against water, moisture, etc.
- 1.1 mm thickness
-
3M™ VHB™ Tape GPH-160GF
- High Temperature Performance (Up to 230°C)
- 1.6 mm thickness
- Permanent seal against water, moisture, etc.
-
3M™ VHB™ Tape GPH-060GF
- High Temperature Performance (Up to 230°C)
- 0.6 mm thickness
- Permanent seal against water, moisture, etc.
-
3M™ VHB™ Tape 5925F
- Double sided acrylic foam tape
- 0.6 mm thickness
- Excellent adhesion to multiple substrates
-
-
3M SJ3540
- Black, interlocking mushroom-shaped heads (250 stem density per square inch)
- Mates with Type 170, Type 250 or Type 400 stem densities
- Strong fastener secures with an audible snap, verifying closure
-
3M™ Dual Lock™ Reclosable Snap Tape SJ3550CF
- Black, interlocking mushroom-shaped heads (250 stem density per square inch)
- Mates with Type 170, Type 250 or Type 400 stem densities
- Clear, acrylic, tape bonds well to a variety of substrates
-
3M™ Dual Lock™ Resealable Snap Tape SJ3560
- Clear, interlocking mushroom-shaped heads (250 stem density per square inch)
- Mates with Type 170, Type 250 or Type 400 stem densities
- Clear, acrylic, tape bonds well to a variety of substrates
-
3M™ Dual Lock™ Resealable Click Strap SJ3870
- Black, interlocking mushroom-shaped heads (250 stem density per square inch)
- Mates with Type 170, Type 250 or Type 400 stem densities
- Black, modified acrylic
-
3M™ Dual Lock™ Resealable Snap Tape SJ3540D
- Black, interlocking mushroom-shaped heads (250 stem density per square inch)
- Mates with Type 170, Type 250 or Type 400 stem densities
- Features good temperature resistance of 120°F (49°C)
-
3M™ Dual Lock™ Resealable Snap Tape SJ3551CF
- Black, interlocking mushroom-shaped heads (400 stem density per square inch)
- Mates with Type 170 and Type 250 stem densities
- Strong fastener secures with an audible snap
-
3M™ Dual Lock™ Resealable Snap Tape SJ387B
- Black, interlocking mushroom-shaped heads (250 stem density per square inch)
- Mates with Type 170, Type 250 or Type 400 stem densities
- Strong fastener secures with an audible snap, verifying closure
-
3M™ Resealable Loop and Hook Fastener SJ352D
- Provide a firm adhesive bond to a wide variety of surfaces
- Durable for thousands of closures
- Best suited for indoor use
-
Scotch® ATG Transfer Tape Gun ATG700
- Automatic liner rewind minimizes waste and eliminates cleanup
- One-handed, trigger-controlled operation supports fast and consistent application
- Delivers uniform adhesive thickness without oozing, glue lines, or overspray
-
3M 260
- Fast curing
- Excellent electrical properties
- Excellent flow • UL 1446 Electrical Insulation System (EIS) approval at class 120(E), 130(B), 155(F), and 180(H)
-
3M Electrically Conductive Double-Sided Tape 9793KW Series
- 0.02-0.20 ohm under 3M ETM-12 test conditions
- Typical expected shielding effectiveness of 40-60 dB
- Broad thickness and adhesion selection
-
3M Electrically Conductive Double-Sided Tape 9793KT Series
- Typical Z-axis electrical resistance`
- Typical expected shielding effectiveness is 40-60 dB
- Ten thicknesses from 130 to 500 µm
-
3M EMI Absorber & Magnetic Shielding Material AB3000 Series
- Broadband 1-10 GHz EMI Absorption
- Configurable Thickness & Adhesive Options
- Die-Cuttable Sheet Format
-
-
3M™ Scotch-Weld™ Structural Adhesive Film AF 30
- Thermosetting Structural Adhesive Film
- 5, 10, and 12 mil Thicknesses
- Flexible Extremely-Low-Flow Film
-
3M™ Scotch-Weld™ Structural Adhesive Film AF 3109-2U
- High-Strength Structural Bonding
- High- and Moderate-Tack Film Options
- 60-Minute 250 deg F Cure
-
3M 1099
- Medium-Viscosity Application Control
- Long-Term Durability by Resisting Weathering
- Adhesion-Promoting Surface Treatment
-
-
3M 30NF
- Water-Dispersed Contact Adhesive
- Heat-Resistant Laminate Bonding
- Greenguard-Certified Wood and Laminate Bonding
-
3M 427
- Dead-Soft Aluminum Foil Backing
- Moisture-Barrier Tape Applications
- -54 to 149 deg C Temperature Resistance
-
3M 467 MP
- 0.06 mm Thin Adhesive Construction
- Peel and Shear on High-Energy Surfaces
- Up to 204 deg C Short-Term Exposure
-
-
3M 550FC
- One-Component Fast Moisture Cure
- High Tensile Strength and Modulus
- Water and Salt-Spray Resistance
-
3M 76
- High-Tack Industrial Formulation Excels in One-Surface Bonding
- Polyethylene and Polypropylene Bonding
- Controlled Variable Lace Spray Pattern
-
3M 8417
- Transparent Self-Wound Polyester Film
- Edge-Tear-Resistant Film Backing
- -40 to 93 deg C Exposure Range
-
3M 853
- 0.06 mm Thin Tape Construction
- Solvent-Resistant Tape Adhesive
- Transparent Label-Protection Tape
-
3M 950
- 5 mil Adhesive 300 Construction
- High Initial Adhesion and Holding
- Multi-Substrate Pressure-Sensitive Bonding
-
3M 966
- Up to 232 deg C Short-Term Exposure
- 10,000-Minute Static Shear
- Metal and High-Energy-Plastic Bonding
-
3M CA40H
- Higher-Viscosity Controlled Dispensing
- EPDM, Vinyl, and Aluminum Bonding
- Alignment-Friendly Slower Set Time
-
-
-
-
-
-
-
-
-
-
-
-
-
-
-
-
-
3M 226
- Chemical-Resistant Surface Protection
- Three-Month Outdoor Clean Removal
- Quick-Stick Hand-Tearable Handling
-
-
3M 232
- Immediate High-Hold Adhesion
- Clean Medium-Temperature Removal
- One-Piece Sliver-Resistant Handling
-
3M 233 PLUS
- Conformable Automotive Paint Masking
- Defined ASTM Physical Strength
- Short High-Temperature Exposure
-
3M 2460
- Low-Ridge Precision Paint Lines
- Delicate-Surface Low-Peel Handling
- Twenty-One-Day Outdoor Removal
-
3M 2517
- General-Purpose Web Splicing
- Versatile Hand-or-Machine Handling
- Short High-Temperature Bake Cycles
-
-
-
-
-
-
3M 3302
- Low-Resistance Conductive Bonding
- Conformable EMI/RFI Shielding
- UL 510 Recognized Construction
-
-
3M 34383
- Hand-Tearable Foil Installation
- Vapor-Barrier Sealing Performance
- Broad -40 to 149 deg C Service
-
-
3M 37852
- Reduced-Adhesive Floor Removal
- Fast Secure Surface Coverage
- Contaminant-Trapping Paint-Booth Protection
-
-
-
-
3M 401M
- Fast High-Initial Substrate Grab
- Fast Hand-Tearable Process Handling
- Defined -40 to 65 deg C Service
-
3M 40PR
- Conductive Anti-Static Adhesion
- Visible Static-Control Identification
- 130 deg C Process Exposure
-
3M 4116
- Fast Initial Multi-Substrate Tack
- Breathable Contaminant-Trapping Seal
- High-Density Vibration Damping
-
-
3M 433L
- High-Temperature Heat Shielding
- Conformable Foil Surface Coverage
- Linered Tape for Die-Cutting
-
-
-
3M 470
- Chemical-Resistant Plating Masks
- Conformable Irregular-Surface Coverage
- Clean-Removal Process Masking
-
3M 470L
- Linered Die-Cut Plating Masks
- Chemical-Resistant Process Protection
- Conformable Curved-Surface Masking
-
3M 471
- Conformable Irregular-Surface Marking
- Clean-Removal Paint Masking
- Vivid Abrasion-Resistant Identification
-
-
3M 483
- Stretch-Conformable Irregular-Surface Sealing
- Low Water-Vapor Transmission
- Up to 12-Month Outdoor Removal
-
3M 4905
- Low-Visibility Permanent Fastening
- Immediate Contact-Bond Handling
- High-Strength HSE Substrate Bonding
-
3M 4950
- Immediate No-Cure Assembly Handling
- Firm 1.1 mm Foam Bonding
- High-Surface-Energy Permanent Attachment
-
3M 50
- All-Weather Pipe Corrosion Protection
- Conformable High-Tack Pipe Wrapping
- Primer-Controlled Metal Surface Adhesion
-
3M 510
- Conformable Diamond-Plate Slip Resistance
- Mineral-Coated High-Friction Walking Surface
- Soft-Mallet Irregular-Surface Conforming
-
3M 528
- Blasting-Media Impact Surface Protection
- Clean One-Piece Tape Removal
- Die-Cuttable Paper-Liner Masking Format
-
3M 540
- One-Part Moisture-Cure Joint Sealing
- Elastic >600% Elongation Profile
- 60 to 90 Minute Tack-Free Window
-
3M 560
- Single-Component Bond-and-Seal Application
- Elastic Moisture-Cured Assembly Bonding
- Panel and Body Bonding Fit
-
3M 583
- Controlled Electronic Film Bondlines
- Heat-and-Pressure Thermal Bonding
- PCB Glass-Fabric Splicing Fit
-
-
3M 5952
- 45-Mil Conformable Foam Bonding
- Painted-Surface Permanent Attachment
- Panel and Display Assembly Bonding
-
3M 598X.5MIC
- Fine Cerium Oxide Final Polishing
- Polyester Film for Controlled Finishing
- Fiber-Optic Ferrule Finishing Fit
-
-
3M 665
- Linerless Manual or Automated Dispensing
- Repositionable Mounting with Clean Removal
- Hot-Wire Cuttable Plastic Construction
-
3M 69
- High-Temperature Electrical Insulation
- Glass-Cloth Coil and Motor Wrapping
- No-Heat Adhesive Application
-
3M 70
- Instant Self-Fusing Cable Overwrap
- Class H High-Temperature Insulation
- Arc-Resistant High-Voltage Protection
-
3M 7445
- Gentle Super Fine Surface Cleaning
- Conformable Pad for Delicate Surfaces
- Rust-Free Steel Wool Alternative
-
3M 7447
- Very Fine Aluminum-Oxide Finishing
- Nonwoven Pad for Surface Preparation
- Cleaning, Blending and Light Deburring
-
3M 7448
- Ultra Fine Silicon-Carbide Finishing
- Conformable Access to Irregular Surfaces
- Load-Resistant Long-Life Open Web
-
3M 78
- EPS and Insulation Material Bonding
- Aerosol or Cylinder Spray Delivery
- Foundation and Foam-Core Applications
-
3M 784F
- Fast Medium-Pressure Metal Grinding
- Flexible Wet-or-Dry Belt Grinding
- Grinding Aid for Heat-Sensitive Alloys
-
3M 7880
- Dot-Matrix Printable Polyester Facestock
- Adhesion Across Metals and Plastics
- Moisture- and Chemical-Resistant Labeling
-
3M 79
- Stable Glass-Cloth Coil Insulation
- 600 V Electrical Tape Rating
- High-Temperature Motor and Transformer Use
-
3M 850
- Low-Caliper High-Strength Process Tape
- Quick-Stick Long-Hold Splicing
- Visible or Transparent Marking Options
-
3M 855
- Clean-Removal High-Temperature Masking
- Non-Silicone Adhesive for Repainting
- High-Elongation Composite Bagging Tape
-
3M 8561
- 14-Mil Indoor Erosion Protection
- Conformable Curved-Surface Tape Protection
- Paint-Compatible Removable Acrylic Adhesion
-
3M 8657DL
- Dual-Liner Aircraft Wet-Area Installation
- Tough Polyurethane Fluid-Barrier Protection
- 82 deg C Wet-Area Service
-
3M 865X
- Precision Silica Fiber-Optic Polishing
- Film-Backed Controlled Fine Lapping
- Multiple Formats for Polishing Sequences
-
3M 8671
- Outdoor UV-Resistant Edge Protection
- Acrylic Pressure-Sensitive Protective Layer
- Converted Formats for Leading Edges
-
3M 8672
- UV-Resistant Outdoor Surface Protection
- 8-Mil Conformable Erosion Barrier
- High-Peel Acrylic Surface Adhesion
-
3M 8681HS
- Polyurethane Leading-Edge Erosion Protection
- Conformable Curved-Surface Coverage
- High-Shear Acrylic Attachment
-
3M 890
- High-Strength Filament Reinforcement
- Heavy-Duty Bundling Support
- Industrial Splicing and Securing
-
3M 8934
- Glass-Reinforced Packaging Strength
- Minimal-Rubdown Package Reinforcement
- Transparent Reinforcement Preserves Graphics
-
-
3M 898
- High-Tensile Filament Reinforcement
- Multi-Surface Synthetic-Rubber Adhesion
- Consistent Curl-Resistant Dispensing
-
-
3M 8992L
- Linered Die-Cut Masking Format
- High-Temperature Silicone Masking
- Clean One-Piece Process Removal
-
-
-
3M 9379
- Thin Profile Transfer Bonding
- Clear Low Visibility Construction
- Fuel And Hydraulic Fluid Resistance
-
3M 9472
- High Tack Transfer Bonding
- Converter Friendly Fiber Reinforcement
- Broad Substrate Peel Performance
-
-
-
3M A3-2
- Fast Handling Strength Development
- Controlled Non Sag Placement
- Oily Surface Process Tolerance
-
-
-
3M AC-730
- Non Chromated Corrosion Inhibition
- Flowable And Thixotropic Options
- Selectable Application Life Grades
-
3M AC-770-B-2-3
- Low Density Fuselage Sealing
- Controlled Thixotropic Placement
- Extended Class B Work Life
-
3M AF536
- Smooth Composite Surface Finish
- Optional Lightning Protection Conductor
- Drapeable Repositionable Layup
-
3M CV45F
- Conformable Panel Seam Bonding
- Immediate Pressure Sensitive Handling
- Stress Relaxing Acrylic Foam
-
-
3M EC-1357
- Fast Interior Contact Assembly
- Positioning Time Before Contact
- Flexible Coating Method Selection
-
-
3M EC-3515
- Lightweight Aerospace Void Filling
- Honeycomb Edge Sealing Control
- Flexible Ambient Or Heat Cure
-
-
3M EC-3549
- High Peel Structural Durability
- Impact Resistant Urethane Bonding
- Controlled Sag Resistant Placement
-
-
3M EC-5816
- Flexible Abrasion-Resistant Protection
- Spray Brush or Flow Application
- 30-Minute Tack-Free Drying
-
-
3M EZ250120
- Medium-Set Wood Assembly
- Thin-Bondline Warm Application
- Moisture-Curing One-Part Processing
-
3M EZ250150
- Extended 2 to 4 Minute Open Time
- Aluminum or Glass to Wood or Plastic
- Flexible Cured Adhesive Layer
-
3M PTFE 5490
- Low-Friction Non-Stick Surface
- Flat Extruded PTFE Backing
- Clean-Removal Silicone Adhesive
-
3M RP2110
- Aircraft Erosion-Protection Repair
- Controlled 1:1 Cartridge Dispensing
- Ten-Minute Working Window
-
3M SJ3526N
- Quick Reclosable Hook Attachment
- Rubber PSA for Low-Energy Plastics
- Manual or Automated Installation
-
-
3M SJ5816
- Die-Cut Protective Conversion
- Skid-Resistant Polyurethane Cushioning
- High-Tack PSA Installation
-
-
3M 100
- Short-Term Exposure to 232 deg C
- Metal and High-Surface-Energy Plastic Adhesion
- Low-Outgassing Tape Construction
-
3M 1099L
- Approximately 40-Minute Open Time
- Spray, Brush, or Roller Application
- Water, Oil, and Fuel Resistance
-
-
3M 40
- 0.025 mm Polyester Backing
- Antistatic Handling of Static-Sensitive Electronics
- Temperature Use Up to 130 deg C
-
3M 4412N
- 2.0 mm Sealing-Tape Thickness
- Instantly Paintable Ionomer Backing
- Immediate Seal Without Chemical Cure
-
-
3M 4693
- Approximate 20-Minute Open Bond Time
- Polyolefin and Engineering-Plastic Bonding
- Brush-Applied Room-Temperature Adhesive
-
3M 48
- 3 mil Unfused PTFE Tape
- Typical -268 to 260 deg C Stability
- Five-Year Shelf Life Under Stated Storage
-
3M 5354
- Non-Curing Butyl Sealant Tape
- Low Moisture-Vapor Transmission
- Vertical, Overhead, and Corner Placement
-
-
-
3M 810
- Visually Unobtrusive on Most Paper
- 53% Renewable-Content Backing
- Pen, Pencil, and Marker Writable
-
-
3M 9690
- Dimensionally Stable PET Carrier for Die Cutting
- 3M 300MP+ Acrylic Adhesive
- 121 deg C Short-Term Exposure
-
-
-
3M™ Scotch-Weld™ Acrylic Adhesive DP8507NS
- Toughened
- 10:1 mix ratio
- Excellent shear strength on bare metals, plastics and other materials
-
3M 08682
- Automotive Urethane Adhesion Primer
- Fast-Drying No-Activator Processing
- UV-Blocking Corrosion-Protection Primer
-
-
3M AB7000E Series
- 300 MHz-4 GHz operating range
- With or without adhesive
- -25 to 105°C temperature range
-
-
-
3M 3901
- Low-Viscosity Surface Wetting
- Quick-Drying One-Component Application
- Improved Metal Corrosion Protection
-
3M AB8000 Series
- Documented near-field EMI absorption from 300 MHz to 4 GHz.
- Four WO magnetic-layer thicknesses from 0.1 to 0.5 mm
- Typical -40 to 150°C temperature range
-
3M™ Hot Melt Adhesive 3748
- High peel
- High temperature performance
- Formulated for bonding low surface energy plastics and coatings
-
-
-
-
3M EC-3901
- Metal And Glass Surface Priming
- Improved Metal Corrosion Protection
- Clean Surface Oxidation Protection
-
-
-
3M™ Hot Melt Adhesive Gun Quadrack™
- Palm trigger reduces hand fatigue during extended dispensing sessions
- Lightweight at 10 oz with glass-reinforced nylon body for industrial durability
- Quadrack feed system accepts 5/8" x 8" Q-size sticks to reduce reloading frequency
-
3M 92
- Polyimide Film with Silicone Adhesive
- 6,000 V Dielectric Breakdown
- UL-Recognized Flame-Retardant Tape
-
3M EC-3924
- Bondline Corrosion Protection
- Spray Brush or Roller Application
- Controlled Film and Bake Process
-
-
3M 3747
- Dissimilar-Substrate Hot-Melt Bonding
- Rapid Strength Development in Seconds
- 45-Second Open Time
-
-
3M DP8610NS
- Flexible Dissimilar Material Bonding
- Non Sag Bondline Control
- Fast Handling Strength Development
-
3M 94
- Enhances adhesion of 3M tapes
- Ideal for low surface energy materials
- Improves bond strength, consistency, and long-term durability
-
-
3M™ VHB™ Surface Cleaner
- Effective degreasing formulation
- For preparation of surfaces for bonding
- Composed of 90% isopropyl alcohol and 10% distilled water
-
3M 3747PG
- Fast Seconds-Scale Bond Set
- Moderate 63 deg C Heat Resistance
- Versatile Plastic-to-Wood Bonding
-
-
-
-
3M 3764-Q
- Quadrack-Format Controlled Dispensing
- Rapid Seconds-Scale Bond Development
- Flexible Impact-Resistant Bond
-
-
-
-
3M 3779TC
- 7,000 cP Melt Viscosity at 191 deg C
- 25-Second Open Time
- 149 deg C Load Resistance at 14 kPa
-
-
3M 3792LM
- 121 to 132 deg C Application Range
- 350 psi Typical Douglas Fir Overlap Shear
- 40-Second Open Time
-
3M 280
- Low-Viscosity Fine-Wire Impregnation
- Semiflexible Cured Performance
- Class F Electrical Insulation
-
3M 281
- Class F (155 deg C) Temperature Rating
- Thermally Conductive Encapsulation
- Upgraded Structural Characteristics
-
-
-
3M DP420
- Bonds metals, composites, glass, ceramics, plastics, and wood
- 20-minute work life at 72°F (22°C) for positioning and alignment before cure
- Handling strength in approximately 2 hours; full cure in 24 hours at room temperature
-
3M DP490
- 90-minute work life supports complex assembly positioning and alignment
- Maintains bond strength across high- and low-temperature operating conditions
- Bonds metals, composites, glass, ceramics, plastics, and wood
-
-
3M 1300L
- Brush or Spray Application
- High Immediate Strength and Heat Resistance
- Metal, Rubber, and Wood Bonding
-
-
3M 847
- Medium-Viscosity Application Control
- Fuel and Oil Resistance
- Adhesion-Promoting Surface Treatment
-
3M 7240FR
- Long open time for large surface application
- Non-sag properties
- Contains glass beads for thickness control
-
-
3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus
- 2-5 minute work life
- Good shear and excellent peel strength
- Flexible
-
3M 760 UV
- High-Modulus, High Shore-a Hardness Formulation
- Moisture-Cure Sealing Processing
- Isocyanate-Free, Low VOC Formulation
-
-
-
3M™ Scotch-Weld™ Epoxy Adhesive 7260FC NS
- Toughened formulation
- Cures at room temperature or accelerated at up to 65 °C
- Working time of 90 minutes
-
3M™ Scotch-Weld™ Epoxy Adhesive 7288
- Two-part A/B epoxy system
- High durability
- Strong adhesion to metals and thermoset plastics
-
-
3M™ Static Mixing Nozzle
- Available for 50 mL and 200 mL / 400 mL cartridge formats
- Doubles as a cartridge storage cap between uses
- Automatic ratio metering through passive cascade mixing
-
3M EPX MIX NOZZLES
- Simultaneous metering, mixing, and application in one step
- Used nozzle doubles as a cartridge storage seal between uses
- Compatible with 3M EPX manual and pneumatic applicators
-
-
3M™ Scotch-Weld™ EPX™ Standard Mixing Nozzle
- Genuine 3M accessory engineered for compatibility with EPX applicators and Duo-Pak cartridges
- Available in configurations for both small-format and larger cartridge systems
- Disposable design eliminates cleanup associated with manual mixing tools
-
-
3M™ Scotch-Weld™ EPX Manual Applicator
- No power source required for portable and in-field operation
- Conversion kits allow support for multiple mix ratios using a single applicator body
- Dual-drive mechanism maintains a consistent mix ratio throughout the dispensing stroke
-
3M 4799
- Flexible EPDM and Rubber Bonding
- Spray, Brush, or Roll Application
- Heat- and Water-Resistant Bond
-
3M™ Scotch-Weld™ EPX Pneumatic Application Gun
- Drip-free dispensing helps minimize material waste and surface contamination
- Integrated regulator enables precise control of adhesive flow rate
- Air-driven dual-piston system maintains accurate mix ratio throughout dispensing
-
3M™ Scotch-Weld™ EPX Structural Adhesive Plunger
- Engineered to precise tolerances for accurate and consistent mix ratio delivery
- Applies even pressure across both cartridge chambers during dispensing
- Enables the EPX Plus II applicator to support multiple cartridge mix ratios
-
-
3M PF5422
- 3.18 mm Preformed Ribbon
- 40 deg F Minimum Application Temperature
- 100% Solids Solvent-Free Sealant
-
3M™ Scotch-Weld™ Structural Adhesive Film AF 163-2 OST Version
- High Structural Bond Strength
- High Fracture Toughness and Peel Strength
- Low-Pressure and Vacuum Curing
-
-
3M DP8625NS
- Flexible Dissimilar Material Bonding
- Controlled Non Sag Dispensing
- Extended Panel Assembly Window
-
-
-
-
-
3M 2216NS
- Flexible Shock/Vibration/Thermal-Cycling Resistance
- High Peel and Shear Strength
- Visual Two-Part Mix Confirmation
-
-
-
-
-
-
3M 49
- High-Solids Water-Based Formula
- Spray, Brush, or Roll Application
- Single-Surface Insulation Bonding
-
3M DP8407NS
- 24.1 MPa Typical 24-Hour Cold-Rolled Steel Overlap Shear
- 5 to 7-Minute Work Life
- 0.010-Inch Glass-Bead Control
-
-
3M DP8405NS
- 10:1 Acrylic Mixing by Volume
- 0.010-Inch Glass-Bead Control
- 18 to 20-Minute Structural Strength
-
-
3M DP8825NS
- 3,000 psi Typical 7-Day Aluminum Overlap Shear
- 22 to 24-Minute Work Life
- 0.010-Inch Glass-Bead Control
-
Scotch-Brite™ Roloc™ SC Surface Conditioning Disc
- Conformable Nonwoven Construction
- Loading Resistance Material
- Quick-Change Attachment System
-
-
3M AF126
- Low Temperature Cure Option
- Low Pressure Structural Bonding
- Selectable Film Weight Construction
-
-
-
3M AF163-2L.0303M
- Lightweight Nonwoven Carrier
- Defined Thin Film Construction
- Low Pressure Cure Capability
-
-
3M AF3028
- Expandable Core Splice Filling
- Low Sag Cure Behavior
- Wide Temperature Structural Performance
-
3M AF325LS.59
- Integrated Composite Surfacing Layer
- Smooth Low Porosity Finish
- Configuration Specific Lightning Protection
-
-
-
3M EC-1751
- Metal Repair And Void Filling
- Controlled Thick Paste Placement
- Flexible Ambient Or Heat Cure
-
3M EC-1838
- Controlled Flow Structural Placement
- One Hour Assembly Work Life
- Durable Environmental Bonding
-
3M EC-2214
- Premixed One Part Processing
- Heat Cured Structural Bonding
- Application Specific Grade Selection
-
3M EC-2216
- Flexible Vibration Resistant Bonding
- High Peel Structural Performance
- Selectable Formulation Processing Window
-
-
3M EC-2815
- Flame Retardant Interior Bonding
- Controlled Honeycomb Insert Placement
- Extended Aerospace Assembly Window
-
3M EC-3439
- Low Density Core Reinforcement
- Extended One Part Shop Life
- High Temperature Cured Performance
-
3M EC-3501
- Rapid Structural Repair Bonding
- Controlled Composite Defect Filling
- High Room Temperature Shear
-
-
3M EC-9300
- Five-Hour Assembly Work Life
- Room-Temperature or Mild-Heat Cure
- Qualified Aircraft Interior FST Data
-
-
-
3M 2290
- Approximately 21% Solids Coating
- Up to Three-Month B-Stage Window
- Multiple Metal-Coating Methods
-
-
-