3M 401 PLUS

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 401

Main features

  • High-temperature performance
  • Clean removal
  • Comfortable crepe paper backing

Product Description

3M™ High Performance Green Masking Tape 401+ is a green crepe paper masking tape designed for critical paint masking applications in automotive, specialty vehicle, and industrial environments. The tape delivers sharp paint lines while helping resist paint edge bleed and provides secure adhesion to a wide range of surfaces, including metal, glass, plastic, rubber, and painted substrates. Its highly conformable crepe paper backing follows curves and contours with ease, while the solvent-free rubber-based adhesive system removes cleanly with minimal residue or slivering. The tape is engineered to withstand short-term temperatures up to 250°F (121°C), making it suitable for paint baking and other elevated-temperature masking processes.

Key features

  • High-temperature performance: Withstands short-term temperatures up to 250°F (121°C) for demanding paint masking operations.
  • Clean removal: Adhesive and backing are designed to minimize residue and slivering during tape removal.
  • Conformable crepe paper backing: Follows curves and contours while maintaining reliable masking coverage.

Applications / Suitable for

  • Automotive paint masking
  • Specialty vehicle finishing operations
  • Industrial paint masking applications
  • High-temperature paint bake processes
  • Masking on metal, glass, plastic, rubber, and painted surfaces

Technical Specifications

General Properties
Color
The color
Green
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
14 %
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
42 N/cm
Other Properties
Storage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical physical and handling properties for the tape in its supplied condition.

Property Value Unit Method / condition
Color Green - As supplied
Adhesive Type Natural / Synthetic Rubber Blend - Product construction
Total Tape Thickness 0.16 mm ASTM D3652
Standard Roll Length 55 m Standard size
Technical properties

After-processing / final-state properties

Typical performance characteristics reported by 3M.

Property Value Unit Method / condition
180° Peel Adhesion 3.8 N/cm ASTM D3330, 23°C, 304 mm/min
Elongation at Break 14 % ASTM D3759
Tensile Strength 42 N/cm ASTM D3759
Short-Term Temperature Resistance 121 °C Short-term exposure