3M 9485PC

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

3M™ Transfer Tape 9485PC

Main features

  • Utilizes a fiber-reinforced adhesive for roll stability
  • Resistance to humidity, water, solvent, and chemicals
  • The 5 mil (127µm) thick version of 3M™ Adhesive Transfer Tape 9482PC

Product Description

3M™ Adhesive Transfer Tape 9485PC is a 5 mil (0.127 mm) high-performance adhesive transfer tape featuring 3M™ Acrylic Adhesive 350, designed for applications requiring high shear strength and elevated temperature performance. Mounted on a tan, 58 lb polycoated kraft (PCK) paper liner, it offers excellent moisture resistance and minimizes wrinkling during application. The fiber-reinforced adhesive enhances roll stability, making it especially suitable for narrow-width applications and bonding both high and low surface energy materials.

Product Key Features

  • Utilizes 3M™ Acrylic Adhesive 350 for strong, reliable bonding
  • Effectively bonds both high surface energy (HSE) and low surface energy (LSE) materials
  • Performs well in elevated temperature conditions
  •  Resistant to oils, gasoline, mild acids, alkalis, and humidity
  • 58 lb polycoated kraft liner reduces wrinkling and provides moisture resistance
  • Suitable for bonding rough and irregular surfaces

Applications

  • Bonding high and low surface energy materials, including powder-coated paints
  • Foam bonding to low surface energy substrates
  • Gasketing and sealing applications
  • Labeling and nameplate attachment
  • Narrow-width and automated dispensing processes
  • General industrial bonding requiring high strength and temperature resistance
Product Family

234908

50 mm x 55 m, 5 pieces
1. Select Width
2. Select Length

Loading pricing…

Product availability
EU Shipping in 2 weeks
Packaging
Unit of measure Roll
Net weight 149.88 kg
Gross weight 149.88 kg
Dimensions 15 x 16 x 5.34 cm

Technical Specifications

General Properties
Color
The color
Translucent
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
127 μm