3M™ Scotch-Weld™ Epoxy Adhesive DP760

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M™ Scotch-Weld™ Epoxy Adhesive DP760

Main features

  • 2:1 mix ratio
  • Non sagging paste
  • High temperature resistance

Product Description

3M Scotch-Weld™ DP760 epoxy adhesive is a non-sag, two-part room temperature curing adhesive designed for use when high temperature resistance is required.

Product Key Features

  • Epoxy adhesive
  • 2:1 mix ratio
  • Non sagging paste for an ease of use
  • High temperature resistance

Applications

  • Powder Coating & Baking Lines: Bonding metal components that must withstand high-temperature curing ovens.
  • Engine Compartment Assembly: Securing brackets, sensors, and structural components near high-heat automotive or aerospace zones.
  • Industrial Oven Fabrication: Sealing joints and mounting hardware on commercial heating equipment.
  • Metal Component Manufacturing: Replacing mechanical fasteners or welding in specialized heavy machinery prone to intense operational heat.
Product Family

234869

White, 50 ml
1. Select Package Type
2. Select Color

Loading pricing…

Product availability
EU Shipping in 2 weeks
Packaging
Unit of measure Cartridge
Net weight 0.076 kg
Gross weight 0.076 kg
Dimensions 4.61 x 2.57 x 12.05 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Modified Epoxy/Modified Amine
Color
The color
White
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
100:50
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.84 - 1.24
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
1.5 hours
Physical Properties
Thixotropic index
Thixotropic Index is a ratio of a material s viscosity at two different speeds in Ambient temperature, generally different by a factor of ten. A thixotropic material s viscosity will decrease as agitation or pressure is increased. It indicates the capability of a material to hold its shape. Mayonnaise is a great example of this. It holds its shape very well, but when a shear stress is applied, the material easily spreads. It helps in choosing a material in accordance to the application, dispense method and viscosity of a material.
Non-sagging Paste

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers