3M 233 PLUS

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 233

Main features

  • Conformable Automotive Paint Masking
  • Defined ASTM Physical Strength
  • Short High-Temperature Exposure

Product Description

Scotch Masking Tape 233 is a smooth mini-crepe paper masking tape with a proprietary rubber-based adhesive for automotive refinish paint masking. Its balanced construction combines instant adhesion and holding power with conformability around curves and controlled handling during application. Typical physical data include 8.0 mil (0.20 mm) thickness, 30 lb/in tensile strength, and 12% elongation at break. The tape resists solvent and moisture, provides clean removal under supported conditions, and tolerates up to 250 deg F (121 deg C) for 30 minutes. It is used for masking cars, airplanes, boats, and trucks where crisp paint lines and reliable edge control are required.

Key features

  • Conformable mini-crepe backing: The smooth paper backing follows curves and contours while supporting controlled hand application.
  • Defined physical strength: Typical tensile strength is 30 lb/in with 12% elongation at break under ASTM D3759.
  • Short high-temperature exposure: The tape tolerates up to 250 deg F (121 deg C) for up to 30 minutes.

Applications

Applications include automotive refinish paint masking on cars, airplanes, boats, and trucks.

Technical Specifications

Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
10 %
Thermal Properties
Temperature Range
Up to 121 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Physical values are typical unless the method / condition states otherwise.

PropertyValueUnitMethod / condition
BackingSmooth mini-crepe paper-As supplied
AdhesiveProprietary rubber-based-As supplied
Total thickness8.0 (0.20)mil (mm)Typical; ASTM D3652
Tensile strength30lb/in widthTypical; ASTM D3759
Elongation at break12%Typical; ASTM D3759
Shelf life12monthsFrom manufacture; original carton at 60 to 80 deg F and 50% RH
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
Adhesion to steel40oz/in widthTypical; ASTM D3330
Temperature useUp to 250 (121)deg F (deg C)Up to 30 min
Clean-removal periodUp to 5daysApplied tape
Solvent and moisture resistanceGood-Applied tape backing