3M DP8010
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Ability to structurally bond polyolefins without special surface preparation
- Excellent water and humidity resistance
- One step process
Product Description
3M™ Scotch-Weld™ Structural Plastic Adhesive DP8010 Blue is a high-performance, two-part acrylic structural adhesive specifically engineered to bond low surface energy plastics, including polypropylene (PP), polyethylene (PE), HDPE, LDPE, UHMW-PE, and thermoplastic olefins (TPO), without the need for special surface preparation. Designed to eliminate the complexity of flame treatment, plasma treatment, primers, and chemical etching, DP8010 provides a simple one-step bonding solution for difficult-to-bond plastics while also delivering excellent adhesion to metals, composites, and dissimilar substrates.
Available in both regular and non-sag formulations, the adhesive offers an 8-minute work life, 10-minute open time, handling strength in approximately 60 minutes, and full cure within 24 hours at room temperature. Its excellent water, humidity, and chemical resistance make it an ideal replacement for mechanical fasteners, rivets, and plastic welding in demanding industrial, transportation, consumer product, and assembly applications.
Key Features
-
Bonds polypropylene (PP), polyethylene (PE), HDPE, LDPE, UHMW-PE, and TPO without special surface preparation.
-
Eliminates primers, chemical etchants, flame treatment, and plasma treatment in many applications.
-
Two-part acrylic structural adhesive with a 10:1 mix ratio.
-
Available in regular (DP8010) and non-sag (DP8010NS) formulations.
-
Excellent adhesion to dissimilar substrates including plastics, metals, and composites.
-
8-minute work life and 10-minute open time for assembly flexibility.
-
Handling strength achieved in approximately 60 minutes.
-
Full room-temperature cure in 24 hours.
-
Excellent water and humidity resistance for durable long-term performance.
-
Very good chemical resistance against many industrial fluids and environmental exposures.
-
Solvent-free adhesive system for simplified processing.
-
Can replace screws, rivets, plastic welding, and multi-step bonding processes.
-
Suitable for automotive plastics, industrial assemblies, appliance components, transportation equipment, composite structures, signage, recreational products, plastic fabrication, and plastic-to-metal bonding applications.
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Additional Information
3M™ Scotch-Weld™ DP8010 Blue / DP8010NS Blue: Structural Adhesive for Low Surface Energy Plastics
3M™ Scotch-Weld™ Structural Plastic Adhesive DP8010 Blue and DP8010NS Blue are two-part acrylic-based adhesives designed to structurally bond many low surface energy plastics, including polypropylene, polyethylene, and TPOs, without special surface preparation. These adhesives offer a one-step bonding process that can replace screws, rivets, plastic welding, chemical etching, priming, and other surface treatment methods in many plastic assembly applications.
Structural bonding for difficult plastics — DP8010 Blue and DP8010NS Blue bond polyolefins such as PP, PE, HDPE, and TPO without flame treatment, plasma treatment, or chemical primers.
Available in regular and non-sag formulations, these adhesives cure at room temperature, provide excellent water and humidity resistance, and support bonding of dissimilar substrates in industrial plastic assembly.
Designed for structural plastic bonding — suitable for polypropylene, polyethylene, HDPE, LDPE, TPO, ABS, PVC, acrylic, FRP, metals, and dissimilar substrate assemblies.
DP8010 Blue and DP8010NS Blue provide a solvent-free adhesive system with convenient cartridge dispensing, bulk availability, and strong overlap shear performance on plastics and metals.

Bonds PP, PE & TPO • No Special Surface Prep • 10:1 Mix Ratio • Room Temperature Cure
Features & Benefits
- Bonds low surface energy plastics such as PP, PE, HDPE, and TPO.
- No special surface preparation required for many polyolefin substrates.
- Two-part acrylic adhesive with 10:1 mix ratio.
- Room-temperature cure with handling strength in approximately 60 minutes.
- Excellent water and humidity resistance for durable plastic bonding.
- Very good chemical resistance for demanding industrial environments.
- Solvent-free adhesive system for cleaner processing.
- Regular and non-sag options for horizontal and vertical applications.
Typical Applications
- Polypropylene and polyethylene bonding.
- TPO and low surface energy plastic assembly.
- Dissimilar substrate bonding.
- Plastic-to-metal bonding.
- Plastic component assembly.
- Replacement for screws, rivets, and plastic welding.
- Industrial, transportation, signage, appliance, and molded plastic assemblies.
Solving the Challenge of Bonding Polyolefins
Low surface energy plastics such as polypropylene and polyethylene are difficult to bond with conventional adhesives because their surfaces resist wetting and adhesion. 3M™ Scotch-Weld™ DP8010 Blue and DP8010NS Blue are designed to bond these plastics without separate flame treatment, plasma treatment, chemical etching, or priming steps, helping simplify production and reduce assembly complexity.
Engineering Data for DP8010 Blue and DP8010NS Blue
| Property | DP8010 Blue | DP8010NS Blue |
|---|---|---|
| Chemistry | Two-part acrylic adhesive | Two-part acrylic adhesive |
| Formulation Type | Regular | Non-sag |
| Color, Mixed | Blue-green | Blue-green |
| Mix Ratio | 10:1 by volume or weight | 10:1 by volume or weight |
| Work Life | Approx. 8 minutes | Approx. 8 minutes |
| Open Time | 10 minutes | 10 minutes |
| Handling Strength | 60 minutes | 60 minutes |
| Full Cure Time | 24 hours | 24 hours |
| Dispense Viscosity | 25,000 cP | 64,000 cP |
| Shore D Hardness | 55–60 | 55–60 |
| Tensile Strength | 1300 psi | 1300 psi |
| Strain at Break | 90% | 90% |
| Glass Transition Temperature | 61 °C | 61 °C |
*Typical properties are representative only and should not be used for specification purposes. Bond performance should be validated under actual substrate, surface preparation, bondline, and environmental conditions.
Typical Overlap Shear Performance
| Substrate | DP8010 Blue | DP8010NS Blue |
|---|---|---|
| Polypropylene, PP | 1150 psi | 1150 psi |
| HDPE | 1040 psi | 1100 psi |
| PVC | 1730 psi | 1740 psi |
| ABS | 1250 psi | 1240 psi |
| Aluminum | 1960 psi | 1780 psi |
| FRP Epoxy | 2830 psi | 2860 psi |
Where DP8010 Blue / DP8010NS Blue Fits
- Polypropylene
- Polyethylene
- TPO and HDPE
- Plastic-to-metal
- Composite bonding
- Mixed-material assemblies
- Cartridge dispensing
- Bulk dispensing
- Fixture-and-cure assembly
Mixing, Application & Cure
Mixing
Use a 10:1 mix ratio by volume or weight. EPX static mixing nozzles are recommended for cartridge use; hand mixing should continue after uniform color is achieved.
Application
Apply adhesive and join surfaces within the open time. Optimum bondline thickness is typically 0.005 to 0.020 inch.
Curing
Allow the adhesive to cure at 60 °F / 16 °C or above. Heat up to 150 °F / 66 °C can increase cure speed.
How DP8010 Simplifies Plastic Assembly
| Assembly Challenge | DP8010 Benefit |
|---|---|
| Polyolefins are difficult to bond with conventional adhesives. | Bonds many PP, PE, HDPE, and TPO substrates without special surface preparation. |
| Mechanical fasteners add weight, holes, and assembly steps. | Can replace screws, rivets, and plastic welding in many plastic assemblies. |
| Vertical or overhead applications require non-sag behavior. | DP8010NS Blue provides a non-sag option for controlled adhesive placement. |
| Assemblies may see humidity, water, and chemical exposure. | Provides excellent water and humidity resistance and very good chemical resistance. |
Ready to Evaluate 3M™ Scotch-Weld™ DP8010?
```