3M 4026
Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.
Main features
- Provides strong holding power for long-term performance
- Maintains bond integrity under elevated temperatures
- Adapts to uneven or irregular surfaces
Product Description
3M™ Double Coated Urethane Foam Tape 4026 is a conformable foam tape designed for mounting, joining, and holding applications across a variety of surfaces. It features a high-temperature acrylic adhesive system that provides strong shear performance and reliable bonding. The urethane foam core allows the tape to conform to irregular surfaces, ensuring consistent contact and durability. Available in roll form and die-cut pieces, this tape offers flexibility for both general and precise applications.
Product Key Features
- Provides strong holding power for long-term performance
- Maintains bond integrity under elevated temperatures
- Adapts to uneven or irregular surfaces for better contact
- Suitable for mounting, joining, and holding across multiple surface types
- Available in rolls and die-cut shapes for application efficiency
- Die-cut pieces available as individual units or pads for quick use
- Foam may turn light yellow when exposed to UV; this does not affect performance
Applications
- General mounting and joining of components
- Holding and positioning parts during assembly
- Use on uneven or irregular surfaces requiring conformability
- Die-cut applications for precise placement (e.g., squares, pads)
- Industrial and general-purpose bonding tasks across various materials
Packaging
Unit of measure Roll
Net weight 0.579583 kg
Gross weight 0.579583 kg
Dimensions 16.2 x 16.2 x 2 cm
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Color
Natural
The color
Total Thickness
1600 μm
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.