TG 3000I | Thermal Grease

Harmonization Code : 3824.99.96.99 | Prepared binders for foundry moulds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included : Other : Other: Other

TG3000I | Thermal Grease

Main features

  • 0.003 Thermal Impedance
  • 3.0 Thermal Conductivity
  • 7μm BLT

Product Description

TG3000I Thermal Silicone Grease is the best thermal grease of our entire product line. It offers excellent thermal properties (3.0 TC and 0.003 TI) while also exhibiting excellent electrical properties. TG3000I has a maximum particle size of 7um and can reach a bond line thickness of 7 micron @35psi, 50oC.  Its low viscosity and excellent thixotropy make it fit for large–scale production with dispensing, screen printing and stencil printing. Even though TC is seemingly average, the combination of Thermal impedance and minuscule bond line thickness along with its great electrical properties, make it the most advanced thermal grease in the market.

TG3000I is used for applications with highly advanced power density requirements. It is designed to minimize thermal resistance at interfaces, and maintain excellent performance through reliability testing. It provides superior thermal performance with ease of use across a multitude of applications.  Its operating temperature range is -40oC to 150oC like the entire Thermal grease product range.

Key Features

  • High-performance thermal grease for advanced power-density designs
  • Thermal conductivity of 3.0 W/m·K with ultra-low thermal impedance of 0.003 °C·in²/W
  • Thin bondline (~7 µm @ 35 psi, 50 °C) enabled by < 7 µm particle size
  • Excellent electrical insulation (2.0 × 10¹² Ω·cm)
  • Low viscosity and thixotropic for smooth dispensing, screen printing, or stencil printing
  • UL 94 V-0 flammability rating for safety in critical assemblies
  • Stable –40 °C to 150 °C operating range
  • Cost-effective and reliable under thermal cycling and long-term stress


Typical Applications

  • Flip-chip BGAs and CPUs
  • Power devices and IGBT modules
  • LED assemblies and drivers
  • GPUs and high-power ASICs
  • Automotive power units and ECUs
  • Telecommunication and data center electronics


 

Product Family

233536

1Kg Jar - 10661494
1. Select Package Type

Loading pricing…

Product availability
EU Shipping in 8 weeks
Packaging
Unit of measure Jar
Net weight 1 kg
Gross weight 1.1 kg
Dimensions 10 x 8 x 8 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
White
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
3.4
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
3.0 W/m.K
Thermal Impedance
0.003 °C·cm²/W
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V-0
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
2000000000000 Ohms⋅cm
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
200,000 mPa.s

Additional Information

Property Nominal Value Permissible Range / Tolerance Test Method / Notes
Thermal Conductivity 2.9 W/m·K 2.7 – 3.3 W/m·K Hot Disk Method
Thermal Impedance 0.003 °C·in²/W — —
Viscosity 339,600 cps @ 25 °C 150,000 – 350,000 cps Brookfield Viscometer
Specific Gravity 3.4 ± 0.1 ASTM D792
Volume Resistivity 2.0 × 10¹² Ω·cm ± 10 % ASTM D257
Flammability V-0 — UL 94
Operating Temperature Range –40 °C to 150 °C — —
Shelf Life 12 months (min.) — Room Temperature Storage
Bond Line Thickness 7 µm @ 35 psi, 50 °C ± 1 µm Internal Method
Maximum Particle Size 7 µm — Internal QC Standard
Format Grease — —
Color White — Visual Inspection


Will I have any issues with fretting(friction) with Greases?

After conducting a thermally degrading test you might realise that these greases are highly filled(~93.5% residual mass). Can this be a cause for concern when it comes to fretting and friction? The short answer is no.

The long answer is that Zinc oxide and aluminum oxide are common fillers in greases and other TIMs. These materials are also used in our phase change TIMs and there has rarely been any issues with fretting (friction) during dispensing or other applications.  Fretting is only a concern with boron nitride as filler.  Friction related impact is also minimal on low viscosity greases. So you are safe.