PLEXUS MA422
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- 10:1 Controlled Mixing
- 17 to 20-Minute Working Window
- 0.75 to 9.5 mm Gap Range
Product Description
PLEXUS® MA422 Methacrylate Adhesive is a two-part, 10:1 methacrylate structural adhesive for bonding composite, thermoplastic, and metal assemblies. The blue, non-sag mixed system provides a typical 17 to 20 minute working time at 23°C and reaches approximately 75% of ultimate strength in 35 to 40 minutes under the documented conditions. It supports bondline gaps from 0.75 to 9.5 mm and is documented for transportation, marine, and industrial assembly applications where a controlled work window and gap-filling bond are required.
Key features
- 17 to 20-minute working time: The documented process window is measured at 23°C.
- Gap-filling structural bond: The adhesive supports documented bondline gaps from 0.75 to 9.5 mm.
- Ductile cured properties: Typical tensile strength is 16.8 to 20.5 MPa with 40 to 70% elongation.
Applications / Suitable for
- Transportation assemblies
- Marine composite bonding
- Industrial metal, thermoplastic, and composite bonding
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Mechanical Properties
Additional Information
As-supplied / before-processing properties
Typical as-supplied values unless otherwise stated. These values are not sales specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color, Part A | Off-white | N/A | As supplied |
| Color, Part B | Blue | N/A | As supplied |
| Mix ratio | 10:1 | parts by volume | Part A : Part B |
| Mix ratio | 9:1 | parts by weight | Part A : Part B |
| Density, Part A | 0.96 | g/mL | As supplied |
| Density, Part B | 1.06 | g/mL | As supplied |
| Viscosity, Part A | 100,000 to 130,000 | cP | As supplied |
| Working time | 17 to 20 | min | At 23°C |
After-processing / final-state properties
Typical final-state values under the stated conditions. These values are not sales specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Recommended bondline gap | 0.75 to 9.5 | mm | Documented range |
| Hardness | 70 | Shore D | Typical cured value |
| Tensile strength | 16.8 to 20.5 | MPa | ASTM D638 / ISO 527 |
| Tensile modulus | 762 to 1,031 | MPa | Typical cured value |
| Elongation | 40 to 70 | % | Typical cured value |