LOCTITE SI 5145

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE SI 5145

Main features

  • Non corrosive
  • Room temperature vulcanization
  • No slumping

Product Description

LOCTITE® SI 5145 is specifically formulated for bonding, sealing, and coating of electronic devices, especially for military, automotive and industrial electronic. The non-slumping nature of this product makes it ideal for reinforcing and strain relieving delicate components. LOCTITE® SI 5145™ resists weathering, moisture, ozone and retains its properties through severe environments.

LOCTITE® SI 5145 is tested to the lot requirements of Military Specification Mil-A-46146B. This non corrosive, room temperature cure product is typically used in applications up to 200 °C

Product Family

233660

40cc Tube - 88318
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 15 days
Packaging
Unit of measure Tube
Net weight 42 g
Gross weight 85 g
Dimensions 23.1 x 0 x 20.9 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
92 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.14
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.2 W/m.K
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
4000000000000000 Ohms⋅cm
Chemical Properties
Water Absorption
0.01 %

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers