LOCTITE D125

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE D125 F

Main features

  • Low exotherm
  • High speed dispensing
  • Low cure temperature

Product Description

LOCTITE D 125 F is a one-component, heat-curable epoxy adhesive specifically formulated for high-speed dispensing in surface mount technology (SMT) assembly. With its low exotherm and minimal water absorption, LOCTITE D 125 F reduces thermal stress on components while ensuring strong adhesion and process reliability.

This yellow adhesive exhibits excellent non-sag and non-stringing characteristics, enabling precise, clean application for chip capacitors, chip resistors, SOTs, SOICs, and PLCCs. It offers high hot strength and fast curing at low temperatures, making it well-suited for demanding, high-throughput electronic manufacturing.

Applications

  • Surface mount assembly of chip capacitors and resistors
  • Bonding SOTs, SOICs, PLCCs, and other SMT components
  • High-speed, precision dispensing processes
  • Electronics production requiring low cure temperatures and non-sag adhesives
Product Family

233991

30cc [30g] EFD Syringe - 1189499
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 25 days
Packaging
Unit of measure Syringe
Net weight 30 g
Gross weight 51 g
Dimensions 4 x 3 x 11.8 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.275
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
85 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.3 W/m.K
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
1e 14 Ohms⋅cm
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
1750000 mPa.s

Additional Information

Cure Profiles
IR or Convection Conveyor Oven:

  • 20 min @ 100 °C

  • 7 min @ 110 °C

  • 2.5 min @ 120 °C

  • 1.5 min @ 150 °C

Convection Box Oven:

  • 30 min @ 100 °C

  • 20 min @ 110 °C

  • 10 min @ 120 °C

  • 5 min @ 150 °C

*Note: Ramp-up should not exceed 1 °C per second

Thawing

  1. Remove the adhesive from cold storage.

  2. Allow the material to reach room temperature (25 °C) before use.

  3. Do not re-freeze once thawed.

  4. Once thawed, apply using the recommended methods.

Directions for Use

  1.  LOCTITE D125 F can be applied by dispensing, pin transfer, screen or stencil printing.
  2. Equipment set-up and related product information is available from your Henkel Corporation support group.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers