LOCTITE 3128

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE 3128

Main features

  • One component
  • Low temperature cure
  • Bonding heat sensitive components

Product Description

LOCTITE 3128 is a one part, heat curable epoxy designed to cure at low temperature and gives excellent adhesion on a wide range of materials in considerably short time. Typical applications include Memory cards, CCD/CMOS Assemblies and Lid/Cap attach for automotive optical sensors and 3d sensing modules.

LOCTITE 3128 can be successfully used as an Edgebond underfill, particularly suited where low curing temperatures are required for heat sensitive components. This low halogen, high viscosity, heat curable epoxy has a good adhesion to a variety of surfaces and a whopping 3 weeks of pot life.

LOCTITE 3128 has a fairly low CTE and warpage and as such has also been used on finger print sensor encapsulation with positive results. This is a camera/sensor market material so is not expected to pass very harsh reliability requirements.

Recommended cure schedule

  • 20 minutes @ 80°C bondline temperature
  • 60 minutes @ 60 °C bondline temperature

Note: Sufficient time must be added to allow the bond location to reach the desired cure temperature. Curing profiles should be developed for each device.

Technical Specifications

General Properties
Color
Black
Pot Life
21 days
Specific Gravity
1.6
Thermal Properties
Glass Transition Temperature (Tg)
45 °C
Electrical Properties
Volume Resistivity
2.9×10¹⁶ Ohms⋅cm
Mechanical Properties
Elongation
2.3 %
Physical Properties
Viscosity
27,000 mPa.s

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers