LENIUM GS

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

VANTAGE LENIUM GS VAPOR SOLVENT

Main features

  • Stabilized nPB Vapor Degreasing
  • Multi-Soil Precision Cleaning
  • Aerospace Solvent-Replacement Approvals Available

Product Description

VANTAGE LENIUM™ GS Vapor Degreasing Solution is a stabilized n-propyl bromide (nPB)-based vapor degreasing solvent designed for use in open-top and vacuum vapor degreasers. It effectively removes adhesives, buffing compounds, drawing oils, greases, hydraulic oils, lapping compounds, resins, inks, silicone oils, and waxes from metal components. LENIUM™ GS serves as a drop-in replacement for trichloroethylene (TCE), HCFC-141b, HCFC-225, perchloroethylene (PCE), and methylene chloride (MeCl), making it suitable for precision cleaning and aerospace surface treatment applications. :contentReference[oaicite:0]{index=0}

Key Features

  • Stabilized nPB formulation for open-top and vacuum vapor degreasing systems.
  • Removes a wide range of industrial soils, including adhesives, oils, greases, resins, inks, silicone oils, and waxes.
  • Drop-in replacement for TCE, HCFC-141b, HCFC-225, PCE, and methylene chloride cleaning processes.

Applications / Suitable for

  • Precision metal cleaning
  • Aerospace component cleaning
  • Open-top vapor degreasing systems
  • Vacuum vapor degreasing systems
  • Removal of machining oils, greases, adhesives, resins, silicone oils, inks, and waxes
Product Family

LENIUM GS

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
105 °C
General Properties
Appearance
Appearance at room temperature.
clear liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.32
Vapor Pressure
110.8 mmHg
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
0.49 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Appearance Clear liquid — As supplied
Specific Gravity (25°C) 1.32 — 25°C
Viscosity (25°C) 0.49 cP 25°C
Vapor Pressure (20°C) 110.8 mm Hg 20°C
Vapor Density (20°C) 3.4 — 20°C
Flash Point None — Published property
Boiling Point 71 (160) °C (°F) Published property
Specific Heat (25°C) 0.27 cal/g·°C 25°C
Heat of Vaporization 58.8 cal/g Published property
Kauri-Butanol (KB) Value 125 — Published property