ENTHONE M SERIES

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ENTHONE M Series

Main features

  • Five-Method Permanent Marking
  • One to 24-Hour Pot-Life Options
  • Humidity-Conditioned Electrical Insulation

Product Description

ENTHONE M-Series Inks are permanent, two-component epoxy marking inks for electronic and industrial identification. The family adheres to glass, metal, and thermosetting plastics when properly applied and cured, and supports hand stamping, machine marking, screen printing, spraying, and roller printing. Catalyst choices provide ambient or heat-cure routes with pot lives from 1 hour to 24 hours, depending on the selected catalyst. Cured films provide chemical and thermal resistance, while color-specific insulation resistance is characterized before and after humidity conditioning. Applications include semiconductor components, printed circuit boards, connectors, dials, nameplates, panels, chassis, glass, and thermoplastics.

Key features

  • Five Marking Methods: Hand stamping, machine marking, screen printing, spraying, and roller printing support varied processes.
  • Ambient or Heat Cure: Catalyst selection provides room-temperature and controlled thermal-cure options.
  • Humidity-Conditioned Electrical Data: Insulation resistance is defined before and after 48-hour humidity conditioning.

Applications / Suitable for

  • Semiconductor-component marking
  • Printed circuit boards and connectors
  • Dials, nameplates, panels, and chassis
  • Glass and thermoplastic marking

Technical Specifications

General Properties
Color
The color
Red, yellow, green, blue, white, black
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two Part (Inks / Catalysts)

Additional Information

Technical properties

As-supplied / before-processing properties

Typical processing data for the ENTHONE M-Series family. Catalyst-specific conditions are identified where applicable.

Property Value Unit Method / condition
Standard catalyst addition 5.0 parts by weight Per 100 parts ink; all standard catalysts except Catalyst 5
Catalyst 5 addition 7.5 parts by weight Per 100 parts ink
Induction period 30; 60 min All standard catalysts; Catalyst 5, respectively
Average pot life 1 to 24 max hr Depends on selected catalyst; measured after induction
Shelf life Ink 3; catalysts 2 years From date of manufacture
Screen mesh 180 to 330 mesh count Monofilament polyester fabric
Squeegee hardness 70 to 80 durometer Sharp, nick-free squeegee for screen printing
Technical properties

After-processing / final-state properties

Typical cured-film data for specified colors and cure conditions. Electrical values vary by ink color and cure schedule.

Property Value Unit Method / condition
Recommended cured film thickness 0.7 to 1.4 (0.017 to 0.035) mil (mm) Cured ink film
Initial insulation resistance M 0 N, M 0 NC, and all other colors: >1.0 x 10^12 ohm MIL-I-43553A; cured 30 min at 121 deg C
Insulation resistance after humidity M 0 N: 1.5 x 10^9; M 0 NC and all other colors: >1.0 x 10^10 ohm MIL-I-43553A; 77 +/- 10 deg F and 95% RH for 48 hr; cured 30 min at 121 deg C
Low-outgassing cure condition 30 at 150 min at deg C Extended cure for low-outgassing properties