ENTHONE CAT 20/A
Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other
Main features
- Two-Hour Mixed-Ink Pot Life
- Ambient or Heat Cure
- Permanent Marking Application Flexibility
Product Description
ENTHONE Catalyst 20/A is an ambient- or heat-cure catalyst component for ENTHONE M-Series and 50-Series two-component epoxy marking inks. With the selected ink, the mixture has an average 2-hour pot life after a 30-minute induction period. A room-temperature air cure reaches tack-free condition in approximately 1 to 2 hours and develops over 5 to 7 days, while heat cure is also available. The catalyst supports permanent marking processes for semiconductor components, printed circuit boards, connectors, dials, nameplates, panels, chassis, glass, and compatible plastics.
Key features
- Two-Hour Mixed Pot Life: The ink and Catalyst 20/A mixture has an average 2-hour pot life after induction.
- Ambient or Heat Cure: The selected ink system may cure at room temperature or through a heat-assisted schedule.
- Multi-Method Marking: Compatible inks may be stamped, screen printed, sprayed, brushed, or roller printed.
Applications / Suitable for
- Permanent marking of semiconductor components
- Printed circuit boards, connectors, and dials
- Nameplates, panels, chassis, glass, and compatible plastics
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-supplied / before-processing properties
Typical processing data for Catalyst 20/A used with M-Series or 50-Series epoxy marking inks.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Induction period | 30 | minutes | Ink/catalyst mixture before application |
| Average pot life | 2 | hours | Catalyst 20/A with M-Series or 50-Series ink; begins after induction |
| Tack-free time | 1 to 2 | hours | Room-temperature air cure; depends on ink film thickness |
| Room-temperature cure | 5 to 7 | days | Catalyst 20/A with ENTHONE epoxy marking ink |
| Cure mode | Room temperature or heat | - | Catalyst 20/A may be fully or partially heat cured |
| Catalyst shelf life | 2 | years | From date of manufacture |
| Moisture handling | Keep tightly closed | - | Catalysts are hygroscopic |